N-WG295

- SCHOTT
- N-WG295 - N-WG295
- 厚度
- 2.0
- 反射系数
- 0.9183
λ [nm] | |
---|---|
200 | < 10⁻³ |
210 | < 10⁻³ |
220 | < 10⁻³ |
230 | < 10⁻³ |
240 | < 10⁻³ |
250 | < 10⁻³ |
260 | < 10⁻³ |
270 | 0.002 |
280 | 0.064 |
290 | 0.326 |
300 | 0.639 |
310 | 0.837 |
320 | 0.928 |
330 | 0.963 |
340 | 0.979 |
350 | 0.986 |
360 | 0.989 |
370 | 0.991 |
380 | 0.992 |
390 | 0.993 |
400 | 0.993 |
410 | 0.994 |
420 | 0.994 |
430 | 0.995 |
440 | 0.995 |
450 | 0.995 |
460 | 0.995 |
470 | 0.996 |
480 | 0.996 |
490 | 0.996 |
λ [nm] | |
---|---|
500 | 0.997 |
510 | 0.997 |
520 | 0.997 |
530 | 0.997 |
540 | 0.997 |
550 | 0.998 |
560 | 0.998 |
570 | 0.998 |
580 | 0.998 |
590 | 0.998 |
600 | 0.998 |
610 | 0.998 |
620 | 0.999 |
630 | 0.999 |
640 | 0.999 |
650 | 0.999 |
660 | 0.999 |
670 | 0.999 |
680 | 0.999 |
690 | 0.999 |
700 | 1.000 |
710 | 1.000 |
720 | 1.000 |
730 | 1.000 |
740 | 1.000 |
750 | 1.000 |
760 | 1.000 |
770 | 1.000 |
780 | 1.000 |
790 | 1.000 |
λ [nm] | |
---|---|
800 | 1.000 |
810 | 1.000 |
820 | 1.000 |
830 | 1.000 |
840 | 1.000 |
850 | 1.000 |
860 | 1.000 |
870 | 1.000 |
880 | 1.000 |
890 | 1.000 |
900 | 1.000 |
910 | 1.000 |
920 | 1.000 |
930 | 1.000 |
940 | 1.000 |
950 | 1.000 |
960 | 1.000 |
970 | 1.000 |
980 | 1.000 |
990 | 1.000 |
1,000 | 1.000 |
1,010 | 1.000 |
1,020 | 1.000 |
1,030 | 1.000 |
1,040 | 1.000 |
1,050 | 1.000 |
1,060 | 1.000 |
1,070 | 1.000 |
1,080 | 1.000 |
1,090 | 1.000 |
λ [nm] | |
---|---|
1,100 | 1.000 |
1,110 | 1.000 |
1,120 | 1.000 |
1,130 | 1.000 |
1,140 | 1.000 |
1,150 | 1.000 |
1,160 | 1.000 |
1,170 | 1.000 |
1,180 | 1.000 |
1,190 | 1.000 |
1,200 | 1.000 |
1,250 | 1.000 |
1,300 | 1.000 |
1,350 | 1.000 |
1,400 | 0.999 |
1,450 | 1.000 |
1,500 | 1.000 |
1,550 | 1.000 |
1,600 | 1.000 |
1,650 | 1.000 |
1,700 | 1.000 |
1,750 | 1.000 |
1,800 | 0.999 |
1,850 | 0.998 |
1,900 | 0.996 |
1,950 | 0.995 |
2,000 | 0.993 |
2,050 | 0.991 |
2,100 | 0.986 |
2,150 | 0.983 |
λ [nm] | |
---|---|
2,200 | 0.976 |
2,250 | 0.973 |
2,300 | 0.975 |
2,350 | 0.971 |
2,400 | 0.965 |
2,450 | 0.959 |
2,500 | 0.952 |
2,550 | 0.946 |
2,600 | 0.939 |
2,650 | 0.926 |
2,700 | 0.854 |
2,750 | 0.420 |
2,800 | 0.358 |
2,850 | 0.399 |
2,900 | 0.424 |
2,950 | 0.442 |
3,000 | 0.451 |
3,050 | 0.454 |
3,100 | 0.452 |
3,150 | 0.447 |
3,200 | 0.436 |
3,250 | 0.426 |
3,300 | 0.409 |
3,350 | 0.385 |
3,400 | 0.357 |
3,450 | 0.324 |
3,500 | 0.288 |
3,550 | 0.249 |
3,600 | 0.220 |
3,650 | 0.202 |
λ [nm] | |
---|---|
3,700 | 0.213 |
3,750 | 0.245 |
3,800 | 0.256 |
3,850 | 0.250 |
3,900 | 0.232 |
3,950 | 0.213 |
4,000 | 0.192 |
4,050 | 0.175 |
4,100 | 0.157 |
4,150 | 0.134 |
4,200 | 0.111 |
4,250 | 0.088 |
4,300 | 0.064 |
4,350 | 0.041 |
4,400 | 0.022 |
4,450 | 0.010 |
4,500 | 0.004 |
4,550 | 0.001 |
4,600 | < 10⁻³ |
4,650 | < 10⁻³ |
4,700 | < 10⁻³ |
4,750 | < 10⁻³ |
4,800 | < 10⁻³ |
4,850 | < 10⁻³ |
4,900 | < 10⁻³ |
4,950 | < 10⁻³ |
5,000 | < 10⁻³ |
5,050 | < 10⁻³ |
5,100 | < 10⁻³ |
5,150 | < 10⁻³ |
反射系数 | |
---|---|
Pd | 0.918 |
参考厚度 | |
---|---|
d [mm] | 2 |
折射率 n |
---|
n (296.7 nm) = 1.550 |
nd (587.6 nm) = 1.520 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] | 2.51 |
气泡含量 | |
---|---|
气泡等级 | 1 |
玻转温度 | |
---|---|
Tg [°C] | 565 |
温度系数 | |
---|---|
Tk [nm/°C] | 0.06 |
耐化学性 | |
---|---|
耐污性 | 0 |
耐酸性 | 1.0 |
耐碱性 | 2.0 |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | 7.2 |
α20°C/300°C [10-6/K] | 8.4 |
α20°C/200°C [10-6/K] |