UG2A

- SCHOTT
- UG2A - UG2A
- 厚度
- 3.0
- 反射系数
- 0.9180
λ [nm] | |
---|---|
200 | |
210 | |
220 | |
230 | |
240 | |
250 | |
260 | |
270 | < 10⁻³ |
280 | < 10⁻³ |
290 | < 10⁻³ |
300 | 0.020 |
310 | 0.162 |
320 | 0.409 |
330 | 0.627 |
340 | 0.764 |
350 | 0.841 |
360 | 0.875 |
370 | 0.867 |
380 | 0.779 |
390 | 0.515 |
400 | 0.152 |
410 | 0.013 |
420 | < 10⁻³ |
430 | < 10⁻³ |
440 | < 10⁻³ |
450 | < 10⁻³ |
460 | < 10⁻³ |
470 | < 10⁻³ |
480 | < 10⁻³ |
490 | < 10⁻³ |
λ [nm] | |
---|---|
500 | < 10⁻³ |
510 | < 10⁻³ |
520 | < 10⁻³ |
530 | < 10⁻³ |
540 | < 10⁻³ |
550 | < 10⁻³ |
560 | < 10⁻³ |
570 | < 10⁻³ |
580 | < 10⁻³ |
590 | < 10⁻³ |
600 | < 10⁻³ |
610 | < 10⁻³ |
620 | < 10⁻³ |
630 | < 10⁻³ |
640 | < 10⁻³ |
650 | < 10⁻³ |
660 | < 10⁻³ |
670 | < 10⁻³ |
680 | < 10⁻³ |
690 | 0.004 |
700 | 0.044 |
710 | 0.148 |
720 | 0.270 |
730 | 0.377 |
740 | 0.482 |
750 | 0.497 |
760 | 0.416 |
770 | 0.325 |
780 | 0.308 |
790 | 0.302 |
λ [nm] | |
---|---|
800 | 0.269 |
810 | 0.229 |
820 | 0.193 |
830 | 0.164 |
840 | 0.141 |
850 | 0.123 |
860 | 0.117 |
870 | 0.109 |
880 | 0.101 |
890 | 0.092 |
900 | 0.090 |
910 | 0.087 |
920 | 0.084 |
930 | 0.082 |
940 | 0.079 |
950 | 0.077 |
960 | 0.075 |
970 | 0.073 |
980 | 0.071 |
990 | 0.068 |
1,000 | 0.064 |
1,010 | 0.061 |
1,020 | 0.056 |
1,030 | 0.052 |
1,040 | 0.047 |
1,050 | 0.043 |
1,060 | 0.038 |
1,070 | 0.035 |
1,080 | 0.031 |
1,090 | 0.028 |
λ [nm] | |
---|---|
1,100 | 0.025 |
1,110 | 0.023 |
1,120 | 0.021 |
1,130 | 0.019 |
1,140 | 0.017 |
1,150 | 0.016 |
1,160 | 0.015 |
1,170 | 0.014 |
1,180 | 0.013 |
1,190 | 0.013 |
1,200 | 0.012 |
1,250 | 0.011 |
1,300 | 0.014 |
1,350 | 0.020 |
1,400 | 0.021 |
1,450 | 0.015 |
1,500 | 0.012 |
1,550 | 0.013 |
1,600 | 0.016 |
1,650 | 0.016 |
1,700 | 0.013 |
1,750 | 0.010 |
1,800 | 0.009 |
1,850 | 0.010 |
1,900 | 0.011 |
1,950 | 0.013 |
2,000 | 0.015 |
2,050 | 0.017 |
2,100 | 0.020 |
2,150 | 0.023 |
λ [nm] | |
---|---|
2,200 | 0.028 |
2,250 | 0.034 |
2,300 | 0.041 |
2,350 | 0.049 |
2,400 | 0.057 |
2,450 | 0.063 |
2,500 | 0.072 |
2,550 | 0.079 |
2,600 | 0.086 |
2,650 | 0.092 |
2,700 | 0.095 |
2,750 | 0.066 |
2,800 | 0.047 |
2,850 | 0.046 |
2,900 | 0.049 |
2,950 | 0.054 |
3,000 | 0.059 |
3,050 | 0.062 |
3,100 | 0.063 |
3,150 | 0.062 |
3,200 | 0.059 |
3,250 | 0.055 |
3,300 | 0.051 |
3,350 | 0.047 |
3,400 | 0.044 |
3,450 | 0.041 |
3,500 | 0.039 |
3,550 | 0.039 |
3,600 | 0.040 |
3,650 | 0.042 |
λ [nm] | |
---|---|
3,700 | 0.045 |
3,750 | 0.050 |
3,800 | 0.055 |
3,850 | 0.061 |
3,900 | 0.068 |
3,950 | 0.073 |
4,000 | 0.074 |
4,050 | 0.071 |
4,100 | 0.064 |
4,150 | 0.055 |
4,200 | 0.046 |
4,250 | 0.038 |
4,300 | 0.030 |
4,350 | 0.022 |
4,400 | 0.015 |
4,450 | 0.008 |
4,500 | 0.004 |
4,550 | 0.002 |
4,600 | < 10⁻³ |
4,650 | < 10⁻³ |
4,700 | < 10⁻³ |
4,750 | < 10⁻³ |
4,800 | < 10⁻³ |
4,850 | < 10⁻³ |
4,900 | < 10⁻³ |
4,950 | < 10⁻³ |
5,000 | < 10⁻³ |
5,050 | < 10⁻³ |
5,100 | < 10⁻³ |
5,150 | < 10⁻³ |
反射系数 | |
---|---|
Pd | 0.918 |
参考厚度 | |
---|---|
d [mm] | 3 |
承诺光谱值 | |
---|---|
τi (303nm) | ≤0.07 |
τi (365nm) | ≥0.81 |
τi (405nm) | ≤0.1 |
τi (694nm) | ≤0.04 |
τi (750nm) | ≤0.52 |
折射率 n |
---|
n (296.7 nm) = 1.567 |
ne (546.1 nm) = 1.525 |
nd (587.6 nm) = 1.523 |
n (302.1 nm) = 1.565 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] | 2.5984 |
气泡含量 | |
---|---|
气泡等级 |
玻转温度 | |
---|---|
Tg [°C] | 484 |
温度系数 | |
---|---|
Tk [nm/°C] |
耐化学性 | |
---|---|
耐污性 | 0.0 |
耐酸性 | 1.0 |
耐碱性 | 1.3 |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | 8.65 |
α20°C/300°C [10-6/K] | 9.94 |
α20°C/200°C [10-6/K] |