BG25

A UV blue bandpass filter that selectively transmits certain wavelength ranges (pass band).

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

BG25
Spectral values guaranteed
τi (334nm) ≤0.8
τi (405nm) ≥0.93
τi (488nm) ≤0.39
τi (725nm) ≤0.36
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
BG25 - BG25
Thickness
1.0
Reflection factor
0.9203
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 0.014
310 0.144
320 0.408
330 0.655
340 0.805
350 0.887
360 0.928
370 0.948
380 0.960
390 0.965
400 0.959
410 0.944
420 0.926
430 0.897
440 0.861
450 0.809
460 0.740
470 0.620
480 0.457
490 0.291
λ [nm]
500 0.183
510 0.097
520 0.045
530 0.017
540 0.010
550 0.015
560 0.025
570 0.018
580 0.005
590 0.001
600 < 10⁻³
610 0.001
620 0.001
630 < 10⁻³
640 < 10⁻³
650 < 10⁻³
660 0.002
670 0.008
680 0.038
690 0.118
700 0.219
710 0.286
720 0.314
730 0.320
740 0.319
750 0.315
760 0.311
770 0.308
780 0.306
790 0.304
λ [nm]
800 0.304
810 0.304
820 0.306
830 0.309
840 0.312
850 0.316
860 0.320
870 0.325
880 0.332
890 0.337
900 0.344
910 0.352
920 0.360
930 0.368
940 0.376
950 0.385
960 0.393
970 0.402
980 0.411
990 0.419
1,000 0.427
1,010 0.434
1,020 0.440
1,030 0.444
1,040 0.448
1,050 0.450
1,060 0.451
1,070 0.450
1,080 0.447
1,090 0.442
λ [nm]
1,100 0.435
1,110 0.426
1,120 0.416
1,130 0.407
1,140 0.392
1,150 0.376
1,160 0.360
1,170 0.345
1,180 0.328
1,190 0.311
1,200 0.294
1,250 0.232
1,300 0.220
1,350 0.250
1,400 0.275
1,450 0.246
1,500 0.230
1,550 0.242
1,600 0.277
1,650 0.298
1,700 0.296
1,750 0.295
1,800 0.313
1,850 0.369
1,900 0.440
1,950 0.515
2,000 0.580
2,050 0.632
2,100 0.670
2,150 0.712
λ [nm]
2,200 0.742
2,250 0.774
2,300 0.800
2,350 0.820
2,400 0.830
2,450 0.836
2,500 0.840
2,550 0.836
2,600 0.832
2,650 0.828
2,700 0.810
2,750 0.725
2,800 0.660
2,850 0.648
2,900 0.647
2,950 0.644
3,000 0.630
3,050 0.608
3,100 0.590
3,150 0.562
3,200 0.530
3,250 0.509
3,300 0.484
3,350 0.464
3,400 0.445
3,450 0.433
3,500 0.423
3,550 0.420
3,600 0.420
3,650 0.423
λ [nm]
3,700 0.426
3,750 0.432
3,800 0.442
3,850 0.452
3,900 0.464
3,950 0.472
4,000 0.477
4,050 0.470
4,100 0.450
4,150 0.430
4,200 0.400
4,250 0.376
4,300 0.340
4,350 0.301
4,400 0.250
4,450 0.205
4,500 0.150
4,550 0.115
4,600 0.078
4,650 0.055
4,700 0.040
4,750 0.033
4,800 0.030
4,850 0.029
4,900 0.026
4,950 0.020
5,000 0.011
5,050 0.005
5,100 0.002
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.920
Reference thickness
d [mm] 1
Spectral values guaranteed
τi (334nm) ≤0.8
τi (405nm) ≥0.93
τi (488nm) ≤0.39
τi (725nm) ≤0.36
Refractive Indices n
nF (486.1 nm) = 1.518
nh (404.7 nm) = 1.527
ng (435.8 nm) = 1.523
ns (852.1 nm) = 1.504
ne (546.1 nm) = 1.514
nd (587.6 nm) = 1.512
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x 0.155 0.151 0.155
y 0.093 0.035 0.024
Y 3 1 0
λd [nm] 470 459 454
Pe 0.90 0.98 0.99
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x 0.153 0.152 0.155
y 0.083 0.033 0.023
Y 3 1 0
λd [nm] 469 458 453
Pe 0.91 0.98 0.99
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x 0.150 0.153 0.157
y 0.055 0.027 0.021
Y 5 2 1
λd [nm] 463 455 451
Pe 0.93 0.98 0.99
Physical values
Density
p [g/cm3] 2.5625
Bubble content
Bubble class
Transformation temperature
Tg [°C] 459
Temperature coefficient
Tk [nm/°C]
Chemical Resistance
FR class 0
SR class 1.0
AR class 1.0
Thermal expansion
α-30°C/+70°C [10-6/K] 8.86
α20°C/300°C [10-6/K] 10.18
α20°C/200°C [10-6/K]