GG400

A longpass filter with low transmission in short wavelengths range and high transmission in long wavelength ranges.

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

GG400
Spectral values guaranteed
λs (τi = 0.00001) [nm] 340
λc (τi = 0.5) [nm] 400 ± 6
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
GG400 - GG400
Thickness
3.0
Reflection factor
0.9183
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 0.003
400 0.491
410 0.859
420 0.908
430 0.926
440 0.936
450 0.945
460 0.952
470 0.958
480 0.964
490 0.969
λ [nm]
500 0.973
510 0.977
520 0.980
530 0.982
540 0.985
550 0.986
560 0.987
570 0.988
580 0.988
590 0.988
600 0.988
610 0.988
620 0.987
630 0.987
640 0.986
650 0.985
660 0.984
670 0.983
680 0.982
690 0.981
700 0.980
710 0.979
720 0.977
730 0.976
740 0.975
750 0.973
760 0.972
770 0.970
780 0.969
790 0.967
λ [nm]
800 0.966
810 0.965
820 0.963
830 0.962
840 0.961
850 0.959
860 0.958
870 0.957
880 0.956
890 0.956
900 0.955
910 0.954
920 0.954
930 0.953
940 0.953
950 0.953
960 0.952
970 0.952
980 0.951
990 0.951
1,000 0.950
1,010 0.950
1,020 0.950
1,030 0.950
1,040 0.950
1,050 0.949
1,060 0.949
1,070 0.949
1,080 0.949
1,090 0.949
λ [nm]
1,100 0.949
1,110 0.949
1,120 0.949
1,130 0.949
1,140 0.949
1,150 0.949
1,160 0.949
1,170 0.950
1,180 0.950
1,190 0.950
1,200 0.950
1,250 0.951
1,300 0.953
1,350 0.956
1,400 0.955
1,450 0.961
1,500 0.965
1,550 0.968
1,600 0.971
1,650 0.972
1,700 0.973
1,750 0.972
1,800 0.970
1,850 0.968
1,900 0.967
1,950 0.965
2,000 0.963
2,050 0.961
2,100 0.957
2,150 0.951
λ [nm]
2,200 0.940
2,250 0.935
2,300 0.940
2,350 0.939
2,400 0.933
2,450 0.923
2,500 0.915
2,550 0.919
2,600 0.908
2,650 0.888
2,700 0.825
2,750 0.344
2,800 0.242
2,850 0.256
2,900 0.274
2,950 0.285
3,000 0.282
3,050 0.276
3,100 0.267
3,150 0.256
3,200 0.238
3,250 0.217
3,300 0.199
3,350 0.186
3,400 0.176
3,450 0.166
3,500 0.159
3,550 0.154
3,600 0.150
3,650 0.149
λ [nm]
3,700 0.154
3,750 0.164
3,800 0.174
3,850 0.181
3,900 0.177
3,950 0.170
4,000 0.163
4,050 0.154
4,100 0.140
4,150 0.127
4,200 0.109
4,250 0.086
4,300 0.060
4,350 0.037
4,400 0.018
4,450 0.008
4,500 0.003
4,550 < 10⁻³
4,600 < 10⁻³
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.918
Reference thickness
d [mm] 3
Spectral values guaranteed
λs (τi = 0.00001) [nm] 340
λc (τi = 0.5) [nm] 400 ± 6
Refractive Indices n
ns (852.1 nm) = 1.520
ne (546.1 nm) = 1.530
nd (587.6 nm) = 1.520
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x 0.448 0.449 0.450
y 0.408 0.409 0.410
Y 91 91 90
λd [nm] 581 581 581
Pe 0.01 0.02 0.03
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x 0.424 0.425 0.426
y 0.400 0.401 0.402
Y 91 91 90
λd [nm] 579 579 579
Pe 0.01 0.02 0.03
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x 0.314 0.315 0.316
y 0.331 0.333 0.335
Y 91 91 90
λd [nm] 570 571 571
Pe 0.01 0.02 0.03
Physical values
Density
p [g/cm3] 2.55
Bubble content
Bubble class 3
Transformation temperature
Tg [°C] 537
Temperature coefficient
Tk [nm/°C] 0.07
Chemical Resistance
FR class 0
SR class 1.0
AR class 1.0
Thermal expansion
α-30°C/+70°C [10-6/K] 7.9
α20°C/300°C [10-6/K] 9.1
α20°C/200°C [10-6/K]