N-WG280

N-WG is a colorless longpass filter with different cutoffs in the UV range, transmitting in the visible and IR ranges.

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

N-WG280
Spectral values guaranteed
λs (τi = 0.00001) [nm] 230
λc (τi = 0.5) [nm] 280 ± 6
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
N-WG280 - N-WG280
Thickness
2.0
Reflection factor
0.9183
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 0.007
260 0.086
270 0.268
280 0.505
290 0.716
300 0.861
310 0.932
320 0.963
330 0.977
340 0.985
350 0.989
360 0.992
370 0.993
380 0.994
390 0.994
400 0.995
410 0.995
420 0.995
430 0.996
440 0.996
450 0.996
460 0.996
470 0.997
480 0.997
490 0.997
λ [nm]
500 0.997
510 0.998
520 0.998
530 0.998
540 0.998
550 0.998
560 0.998
570 0.999
580 0.999
590 0.999
600 0.999
610 0.999
620 0.999
630 0.999
640 1.000
650 1.000
660 1.000
670 1.000
680 1.000
690 1.000
700 1.000
710 1.000
720 1.000
730 1.000
740 1.000
750 1.000
760 1.000
770 1.000
780 1.000
790 1.000
λ [nm]
800 1.000
810 1.000
820 1.000
830 1.000
840 1.000
850 1.000
860 1.000
870 1.000
880 1.000
890 1.000
900 1.000
910 1.000
920 1.000
930 1.000
940 1.000
950 1.000
960 1.000
970 1.000
980 1.000
990 1.000
1,000 1.000
1,010 1.000
1,020 1.000
1,030 1.000
1,040 1.000
1,050 1.000
1,060 1.000
1,070 1.000
1,080 1.000
1,090 1.000
λ [nm]
1,100 1.000
1,110 1.000
1,120 1.000
1,130 1.000
1,140 1.000
1,150 1.000
1,160 1.000
1,170 1.000
1,180 1.000
1,190 1.000
1,200 1.000
1,250 1.000
1,300 1.000
1,350 1.000
1,400 0.999
1,450 1.000
1,500 1.000
1,550 1.000
1,600 1.000
1,650 1.000
1,700 1.000
1,750 1.000
1,800 1.000
1,850 0.999
1,900 0.998
1,950 0.997
2,000 0.996
2,050 0.994
2,100 0.989
2,150 0.986
λ [nm]
2,200 0.981
2,250 0.978
2,300 0.979
2,350 0.976
2,400 0.971
2,450 0.964
2,500 0.958
2,550 0.951
2,600 0.943
2,650 0.926
2,700 0.854
2,750 0.438
2,800 0.415
2,850 0.444
2,900 0.474
2,950 0.488
3,000 0.493
3,050 0.493
3,100 0.490
3,150 0.484
3,200 0.474
3,250 0.462
3,300 0.442
3,350 0.417
3,400 0.389
3,450 0.352
3,500 0.311
3,550 0.271
3,600 0.243
3,650 0.221
λ [nm]
3,700 0.233
3,750 0.261
3,800 0.275
3,850 0.265
3,900 0.246
3,950 0.225
4,000 0.204
4,050 0.184
4,100 0.165
4,150 0.141
4,200 0.116
4,250 0.090
4,300 0.064
4,350 0.041
4,400 0.022
4,450 0.010
4,500 0.004
4,550 0.001
4,600 < 10⁻³
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.918
Reference thickness
d [mm] 2
Spectral values guaranteed
λs (τi = 0.00001) [nm] 230
λc (τi = 0.5) [nm] 280 ± 6
Refractive Indices n
nF (486.1 nm) = 1.523
n (296.7 nm) = 1.550
nh (404.7 nm) = 1.530
ng (435.8 nm) = 1.527
ns (852.1 nm) = 1.510
ne (546.1 nm) = 1.519
nd (587.6 nm) = 1.517
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Physical values
Density
p [g/cm3] 2.51
Bubble content
Bubble class 1
Transformation temperature
Tg [°C] 558
Temperature coefficient
Tk [nm/°C] 0.06
Chemical Resistance
FR class 0
SR class 1.0
AR class 2.0
Thermal expansion
α-30°C/+70°C [10-6/K] 7.1
α20°C/300°C [10-6/K] 8.4
α20°C/200°C [10-6/K]