N-WG320

N-WG is a colorless longpass filter with different cutoffs in the UV range, transmitting in the visible and IR ranges.

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

N-WG320
Spectral values guaranteed
λs (τi = 0.00001) [nm] 280 nm
λc (τi = 0.5) [nm] 320 nm ± 6 nm
λp1 (τi = 0.99) [nm] 470 nm
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
N-WG320 - N-WG320
Thickness
2.0
Reflection factor
0.9183
Internal Transmittance (Table)
λ [nm]
200
210
220
230
240
250
260
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 0.007
310 0.163
320 0.531
330 0.803
340 0.927
350 0.973
360 0.988
370 0.995
380 0.998
390 0.999
400 0.999
410 1.000
420 1.000
430 1.000
440 1.000
450 1.000
460 1.000
470 1.000
480 1.000
490 1.000
λ [nm]
500 1.000
510 1.000
520 1.000
530 1.000
540 1.000
550 1.000
560 1.000
570 1.000
580 1.000
590 1.000
600 1.000
610 1.000
620 1.000
630 1.000
640 1.000
650 1.000
660 1.000
670 1.000
680 1.000
690 1.000
700 1.000
710 1.000
720 1.000
730 1.000
740 1.000
750 1.000
760 1.000
770 1.000
780 1.000
790 1.000
λ [nm]
800 1.000
810 1.000
820 1.000
830 1.000
840 1.000
850 1.000
860 1.000
870 1.000
880 1.000
890 1.000
900 1.000
910 1.000
920 1.000
930 1.000
940 1.000
950 1.000
960 1.000
970 1.000
980 1.000
990 1.000
1,000 1.000
1,010 1.000
1,020 1.000
1,030 1.000
1,040 1.000
1,050 1.000
1,060 1.000
1,070 1.000
1,080 1.000
1,090 1.000
λ [nm]
1,100 1.000
1,110 1.000
1,120 1.000
1,130 1.000
1,140 1.000
1,150 1.000
1,160 1.000
1,170 1.000
1,180 1.000
1,190 1.000
1,200 1.000
1,250 1.000
1,300 1.000
1,350 1.000
1,400 0.996
1,450 0.998
1,500 0.999
1,550 0.999
1,600 0.999
1,650 0.998
1,700 0.998
1,750 0.997
1,800 0.996
1,850 0.995
1,900 0.994
1,950 0.992
2,000 0.991
2,050 0.987
2,100 0.980
2,150 0.977
λ [nm]
2,200 0.971
2,250 0.968
2,300 0.969
2,350 0.968
2,400 0.961
2,450 0.954
2,500 0.946
2,550 0.942
2,600 0.937
2,650 0.928
2,700 0.881
2,750 0.423
2,800 0.347
2,850 0.373
2,900 0.399
2,950 0.420
3,000 0.433
3,050 0.439
3,100 0.440
3,150 0.439
3,200 0.435
3,250 0.429
3,300 0.419
3,350 0.402
3,400 0.378
3,450 0.349
3,500 0.310
3,550 0.270
3,600 0.242
3,650 0.219
λ [nm]
3,700 0.227
3,750 0.258
3,800 0.272
3,850 0.268
3,900 0.251
3,950 0.229
4,000 0.208
4,050 0.191
4,100 0.172
4,150 0.148
4,200 0.121
4,250 0.093
4,300 0.068
4,350 0.046
4,400 0.027
4,450 0.014
4,500 0.006
4,550 0.002
4,600 < 10⁻³
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.918
Reference thickness
d [mm] 2
Spectral values guaranteed
λs (τi = 0.00001) [nm] 280 nm
λc (τi = 0.5) [nm] 320 nm ± 6 nm
λp1 (τi = 0.99) [nm] 470 nm
Refractive Indices n
nF (486.1 nm) = 1.526
nh (404.7 nm) = 1.535
ng (435.8 nm) = 1.531
ns (852.1 nm) = 1.513
ne (546.1 nm) = 1.523
nd (587.6 nm) = 1.521
n (302.1 nm) = 1.558
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Physical values
Density
p [g/cm3] 2.512
Bubble content
Bubble class 1
Transformation temperature
Tg [°C] 563
Temperature coefficient
Tk [nm/°C]
Chemical Resistance
FR class 0
SR class 1.0
AR class 2.0
Thermal expansion
α-30°C/+70°C [10-6/K] 7.1
α20°C/300°C [10-6/K] 8.4
α20°C/200°C [10-6/K]