RG645
Spectral values guaranteed
λs (τi = 0.00001) [nm] 560
λc (τi = 0.5) [nm] 645 ± 6
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
RG645 - RG645
Thickness
3.0
Reflection factor
0.9183
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 < 10⁻³
400 < 10⁻³
410 < 10⁻³
420 < 10⁻³
430 < 10⁻³
440 < 10⁻³
450 < 10⁻³
460 < 10⁻³
470 < 10⁻³
480 < 10⁻³
490 < 10⁻³
λ [nm]
500 < 10⁻³
510 < 10⁻³
520 < 10⁻³
530 < 10⁻³
540 < 10⁻³
550 < 10⁻³
560 < 10⁻³
570 < 10⁻³
580 < 10⁻³
590 < 10⁻³
600 < 10⁻³
610 < 10⁻³
620 0.004
630 0.061
640 0.311
650 0.645
660 0.845
670 0.927
680 0.959
690 0.971
700 0.976
710 0.978
720 0.978
730 0.978
740 0.977
750 0.977
760 0.975
770 0.974
780 0.973
790 0.972
λ [nm]
800 0.971
810 0.970
820 0.969
830 0.968
840 0.967
850 0.966
860 0.966
870 0.965
880 0.965
890 0.964
900 0.964
910 0.964
920 0.963
930 0.963
940 0.962
950 0.962
960 0.962
970 0.961
980 0.961
990 0.961
1,000 0.961
1,010 0.960
1,020 0.960
1,030 0.960
1,040 0.960
1,050 0.960
1,060 0.960
1,070 0.960
1,080 0.960
1,090 0.960
λ [nm]
1,100 0.960
1,110 0.961
1,120 0.961
1,130 0.961
1,140 0.961
1,150 0.961
1,160 0.962
1,170 0.962
1,180 0.962
1,190 0.962
1,200 0.963
1,250 0.964
1,300 0.966
1,350 0.968
1,400 0.969
1,450 0.973
1,500 0.977
1,550 0.979
1,600 0.981
1,650 0.982
1,700 0.981
1,750 0.980
1,800 0.979
1,850 0.977
1,900 0.976
1,950 0.975
2,000 0.974
2,050 0.973
2,100 0.971
2,150 0.968
λ [nm]
2,200 0.955
2,250 0.952
2,300 0.955
2,350 0.956
2,400 0.953
2,450 0.947
2,500 0.941
2,550 0.945
2,600 0.945
2,650 0.934
2,700 0.889
2,750 0.544
2,800 0.392
2,850 0.374
2,900 0.379
2,950 0.378
3,000 0.367
3,050 0.346
3,100 0.318
3,150 0.291
3,200 0.269
3,250 0.248
3,300 0.231
3,350 0.218
3,400 0.208
3,450 0.204
3,500 0.205
3,550 0.211
3,600 0.221
3,650 0.230
λ [nm]
3,700 0.240
3,750 0.250
3,800 0.262
3,850 0.271
3,900 0.279
3,950 0.283
4,000 0.279
4,050 0.266
4,100 0.244
4,150 0.215
4,200 0.184
4,250 0.153
4,300 0.120
4,350 0.085
4,400 0.051
4,450 0.025
4,500 0.012
4,550 0.005
4,600 0.002
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.918
Reference thickness
d [mm] 3
Spectral values guaranteed
λs (τi = 0.00001) [nm] 560
λc (τi = 0.5) [nm] 645 ± 6
Refractive Indices n
ns (852.1 nm) = 1.520
nd (587.6 nm) = 1.520
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x 0.672 0.722 0.726
y 0.303 0.277 0.274
Y 9 5 4
λd [nm] 640 647 651
Pe 0.83 0.99 1.00
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x 0.662 0.722 0.726
y 0.304 0.277 0.274
Y 8 4 3
λd [nm] 640 646 651
Pe 0.81 0.99 1.00
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x 0.584 0.717 0.726
y 0.298 0.278 0.274
Y 5 2 2
λd [nm] 638 645 650
Pe 0.67 0.98 1.00
Physical values
Density
p [g/cm3] 2.65
Bubble content
Bubble class 3
Transformation temperature
Tg [°C] 519
Temperature coefficient
Tk [nm/°C] 0.16
Chemical Resistance
FR class 0
SR class 1.0
AR class 1.0
Thermal expansion
α-30°C/+70°C [10-6/K] 8
α20°C/300°C [10-6/K] 9.2
α20°C/200°C [10-6/K]