RG715

A longpass filter with low transmission in short wavelengths range and high transmission in long wavelength ranges. They seperate visible from infrared light.

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

RG715
Spectral values guaranteed
λs (τi = 0.00001) [nm] 620
λc (τi = 0.5) [nm] 715 ± 9
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
RG715 - RG715
Thickness
3.0
Reflection factor
0.9143
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 < 10⁻³
400 < 10⁻³
410 < 10⁻³
420 < 10⁻³
430 < 10⁻³
440 < 10⁻³
450 < 10⁻³
460 < 10⁻³
470 < 10⁻³
480 < 10⁻³
490 < 10⁻³
λ [nm]
500 < 10⁻³
510 < 10⁻³
520 < 10⁻³
530 < 10⁻³
540 < 10⁻³
550 < 10⁻³
560 < 10⁻³
570 < 10⁻³
580 < 10⁻³
590 < 10⁻³
600 < 10⁻³
610 < 10⁻³
620 < 10⁻³
630 < 10⁻³
640 < 10⁻³
650 < 10⁻³
660 < 10⁻³
670 < 10⁻³
680 < 10⁻³
690 0.005
700 0.059
710 0.311
720 0.666
730 0.866
740 0.941
750 0.967
760 0.976
770 0.979
780 0.980
790 0.981
λ [nm]
800 0.980
810 0.980
820 0.980
830 0.980
840 0.980
850 0.980
860 0.979
870 0.979
880 0.979
890 0.980
900 0.980
910 0.980
920 0.980
930 0.980
940 0.980
950 0.980
960 0.980
970 0.980
980 0.980
990 0.981
1,000 0.981
1,010 0.981
1,020 0.981
1,030 0.981
1,040 0.981
1,050 0.981
1,060 0.981
1,070 0.981
1,080 0.982
1,090 0.982
λ [nm]
1,100 0.982
1,110 0.982
1,120 0.982
1,130 0.982
1,140 0.982
1,150 0.983
1,160 0.983
1,170 0.983
1,180 0.983
1,190 0.983
1,200 0.984
1,250 0.985
1,300 0.986
1,350 0.988
1,400 0.988
1,450 0.990
1,500 0.992
1,550 0.993
1,600 0.993
1,650 0.993
1,700 0.992
1,750 0.990
1,800 0.989
1,850 0.988
1,900 0.987
1,950 0.987
2,000 0.986
2,050 0.985
2,100 0.984
2,150 0.980
λ [nm]
2,200 0.968
2,250 0.964
2,300 0.968
2,350 0.968
2,400 0.966
2,450 0.960
2,500 0.954
2,550 0.959
2,600 0.960
2,650 0.949
2,700 0.902
2,750 0.560
2,800 0.365
2,850 0.338
2,900 0.336
2,950 0.334
3,000 0.324
3,050 0.307
3,100 0.286
3,150 0.266
3,200 0.248
3,250 0.233
3,300 0.220
3,350 0.212
3,400 0.207
3,450 0.209
3,500 0.217
3,550 0.231
3,600 0.248
3,650 0.265
λ [nm]
3,700 0.283
3,750 0.299
3,800 0.313
3,850 0.323
3,900 0.330
3,950 0.330
4,000 0.325
4,050 0.315
4,100 0.299
4,150 0.276
4,200 0.246
4,250 0.212
4,300 0.167
4,350 0.124
4,400 0.080
4,450 0.044
4,500 0.020
4,550 0.008
4,600 0.003
4,650 0.001
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.914
Reference thickness
d [mm] 3
Spectral values guaranteed
λs (τi = 0.00001) [nm] 620
λc (τi = 0.5) [nm] 715 ± 9
Refractive Indices n
nF (486.1 nm) = 1.544
nh (404.7 nm) = 1.554
ng (435.8 nm) = 1.550
ns (852.1 nm) = 1.528
ne (546.1 nm) = 1.539
nd (587.6 nm) = 1.537
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Physical values
Density
p [g/cm3] 2.76
Bubble content
Bubble class 3
Transformation temperature
Tg [°C] 532
Temperature coefficient
Tk [nm/°C] 0.18
Chemical Resistance
FR class 0
SR class 1.0
AR class 1.0
Thermal expansion
α-30°C/+70°C [10-6/K] 8.1
α20°C/300°C [10-6/K] 9.4
α20°C/200°C [10-6/K]