RG850

A longpass filter with low transmission in short wavelengths range and high transmission in long wavelength ranges. They seperate visible from infrared light.

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

RG850
Spectral values guaranteed
λs (τi = 0.00001) [nm] 700 nm
λc (τi = 0.5) [nm] 850 nm ± 9 nm
λp1 (τi = 0.9) [nm] 950 nm
λp2 (τi = 0.97) [nm] 1200 nm
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
RG850 - RG850
Thickness
3.0
Reflection factor
0.9087
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 < 10⁻³
400 < 10⁻³
410 < 10⁻³
420 < 10⁻³
430 < 10⁻³
440 < 10⁻³
450 < 10⁻³
460 < 10⁻³
470 < 10⁻³
480 < 10⁻³
490 < 10⁻³
λ [nm]
500 < 10⁻³
510 < 10⁻³
520 < 10⁻³
530 < 10⁻³
540 < 10⁻³
550 < 10⁻³
560 < 10⁻³
570 < 10⁻³
580 < 10⁻³
590 < 10⁻³
600 < 10⁻³
610 < 10⁻³
620 < 10⁻³
630 < 10⁻³
640 < 10⁻³
650 < 10⁻³
660 < 10⁻³
670 < 10⁻³
680 < 10⁻³
690 < 10⁻³
700 < 10⁻³
710 < 10⁻³
720 < 10⁻³
730 < 10⁻³
740 < 10⁻³
750 < 10⁻³
760 < 10⁻³
770 < 10⁻³
780 < 10⁻³
790 < 10⁻³
λ [nm]
800 0.001
810 0.005
820 0.024
830 0.091
840 0.261
850 0.500
860 0.704
870 0.838
880 0.905
890 0.940
900 0.957
910 0.965
920 0.971
930 0.974
940 0.977
950 0.978
960 0.979
970 0.980
980 0.981
990 0.982
1,000 0.983
1,010 0.984
1,020 0.985
1,030 0.986
1,040 0.987
1,050 0.987
1,060 0.988
1,070 0.989
1,080 0.989
1,090 0.990
λ [nm]
1,100 0.990
1,110 0.991
1,120 0.991
1,130 0.992
1,140 0.992
1,150 0.993
1,160 0.993
1,170 0.994
1,180 0.994
1,190 0.994
1,200 0.995
1,250 0.996
1,300 0.997
1,350 0.998
1,400 0.997
1,450 0.998
1,500 1.000
1,550 1.000
1,600 1.000
1,650 0.999
1,700 0.997
1,750 0.995
1,800 0.993
1,850 0.992
1,900 0.991
1,950 0.989
2,000 0.987
2,050 0.987
2,100 0.984
2,150 0.978
λ [nm]
2,200 0.966
2,250 0.957
2,300 0.958
2,350 0.956
2,400 0.947
2,450 0.941
2,500 0.937
2,550 0.934
2,600 0.927
2,650 0.911
2,700 0.865
2,750 0.509
2,800 0.224
2,850 0.169
2,900 0.142
2,950 0.121
3,000 0.104
3,050 0.093
3,100 0.083
3,150 0.077
3,200 0.074
3,250 0.072
3,300 0.068
3,350 0.064
3,400 0.059
3,450 0.054
3,500 0.049
3,550 0.045
3,600 0.045
3,650 0.045
λ [nm]
3,700 0.042
3,750 0.037
3,800 0.035
3,850 0.042
3,900 0.055
3,950 0.072
4,000 0.071
4,050 0.063
4,100 0.057
4,150 0.052
4,200 0.049
4,250 0.052
4,300 0.051
4,350 0.044
4,400 0.033
4,450 0.023
4,500 0.013
4,550 0.007
4,600 0.003
4,650 0.001
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.909
Reference thickness
d [mm] 3
Spectral values guaranteed
λs (τi = 0.00001) [nm] 700 nm
λc (τi = 0.5) [nm] 850 nm ± 9 nm
λp1 (τi = 0.9) [nm] 950 nm
λp2 (τi = 0.97) [nm] 1200 nm
Refractive Indices n
ns (852.1 nm) = 1.550
nd (587.6 nm) = 1.560
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Physical values
Density
p [g/cm3] 2.93
Bubble content
Bubble class 3
Transformation temperature
Tg [°C] 554
Temperature coefficient
Tk [nm/°C] 0.24
Chemical Resistance
FR class 5
SR class 53.4
AR class 1.3
Thermal expansion
α-30°C/+70°C [10-6/K] 9.41
α20°C/300°C [10-6/K] 10.41
α20°C/200°C [10-6/K]