UG11

A bandpass filter that shows its highest transmission in the UV wavelength ranges (pass band).

Find more information in the tabs below or on our website.

Use our Interactive Filter Diagram to compare this filter or download our Filter Calculation Tool.

For customized filter products you can mark an article and use the request-button.

*product image is exemplary.

UG11
Spectral values guaranteed
τi (254nm) ≥ 0,06
τi (334nm) ≥ 0,9
τi (405nm) ≤ 0,001
τi (694nm) ≤ 0,26
τi (725nm) ≤ 0,32
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 0.1 and 30 with one decimal place are allowed.

SCHOTT
UG11 - UG11
Thickness
1.0
Reflection factor
0.9079
Internal Transmittance (Table)
λ [nm]
200
210
220
230 < 10⁻³
240 < 10⁻³
250 0.056
260 0.276
270 0.521
280 0.712
290 0.825
300 0.880
310 0.907
320 0.920
330 0.926
340 0.921
350 0.906
360 0.866
370 0.756
380 0.482
390 0.120
400 0.004
410 < 10⁻³
420 < 10⁻³
430 < 10⁻³
440 < 10⁻³
450 < 10⁻³
460 < 10⁻³
470 < 10⁻³
480 < 10⁻³
490 < 10⁻³
λ [nm]
500 < 10⁻³
510 < 10⁻³
520 < 10⁻³
530 < 10⁻³
540 < 10⁻³
550 < 10⁻³
560 < 10⁻³
570 < 10⁻³
580 < 10⁻³
590 < 10⁻³
600 < 10⁻³
610 < 10⁻³
620 < 10⁻³
630 < 10⁻³
640 < 10⁻³
650 < 10⁻³
660 < 10⁻³
670 0.008
680 0.050
690 0.138
700 0.222
710 0.278
720 0.283
730 0.240
740 0.185
750 0.136
760 0.097
770 0.067
780 0.047
790 0.033
λ [nm]
800 0.024
810 0.018
820 0.014
830 0.011
840 0.009
850 0.008
860 0.007
870 0.006
880 0.006
890 0.006
900 0.006
910 0.006
920 0.006
930 0.007
940 0.008
950 0.009
960 0.011
970 0.013
980 0.015
990 0.018
1,000 0.021
1,010 0.025
1,020 0.028
1,030 0.033
1,040 0.037
1,050 0.041
1,060 0.044
1,070 0.046
1,080 0.048
1,090 0.048
λ [nm]
1,100 0.049
1,110 0.046
1,120 0.043
1,130 0.039
1,140 0.037
1,150 0.033
1,160 0.030
1,170 0.027
1,180 0.024
1,190 0.021
1,200 0.018
1,250 0.009
1,300 0.005
1,350 0.005
1,400 0.005
1,450 0.005
1,500 0.004
1,550 0.004
1,600 0.005
1,650 0.006
1,700 0.007
1,750 0.007
1,800 0.007
1,850 0.007
1,900 0.008
1,950 0.010
2,000 0.012
2,050 0.016
2,100 0.020
2,150 0.026
λ [nm]
2,200 0.032
2,250 0.038
2,300 0.046
2,350 0.053
2,400 0.060
2,450 0.068
2,500 0.070
2,550 0.070
2,600 0.070
2,650 0.072
2,700 0.070
2,750 0.064
2,800 0.030
2,850 0.011
2,900 0.005
2,950 0.003
3,000 0.002
3,050 0.001
3,100 < 10⁻³
3,150 < 10⁻³
3,200 < 10⁻³
3,250 < 10⁻³
3,300 < 10⁻³
3,350 < 10⁻³
3,400 < 10⁻³
3,450 < 10⁻³
3,500 < 10⁻³
3,550 < 10⁻³
3,600 < 10⁻³
3,650 < 10⁻³
λ [nm]
3,700 < 10⁻³
3,750 < 10⁻³
3,800 < 10⁻³
3,850 < 10⁻³
3,900 < 10⁻³
3,950 < 10⁻³
4,000 < 10⁻³
4,050 < 10⁻³
4,100 < 10⁻³
4,150 < 10⁻³
4,200 < 10⁻³
4,250 < 10⁻³
4,300 < 10⁻³
4,350 < 10⁻³
4,400 < 10⁻³
4,450 < 10⁻³
4,500 < 10⁻³
4,550 < 10⁻³
4,600 < 10⁻³
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.908
Reference thickness
d [mm] 1
Spectral values guaranteed
τi (254nm) ≥ 0,06
τi (334nm) ≥ 0,9
τi (405nm) ≤ 0,001
τi (694nm) ≤ 0,26
τi (725nm) ≤ 0,32
Refractive Indices n
nF (486.1 nm) = 1.569
n (296.7 nm) = 1.606
nh (404.7 nm) = 1.579
ng (435.8 nm) = 1.574
ns (852.1 nm) = 1.556
ne (546.1 nm) = 1.565
nd (587.6 nm) = 1.563
n (302.1 nm) = 1.604
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
Physical values
Density
p [g/cm3] 2.92
Bubble content
Bubble class
Transformation temperature
Tg [°C] 545
Temperature coefficient
Tk [nm/°C]
Chemical Resistance
FR class 0
SR class 3.0
AR class 2.2
Thermal expansion
α-30°C/+70°C [10-6/K] 7.8
α20°C/300°C [10-6/K] 9
α20°C/200°C [10-6/K]