Technical Details
Internal Transmittance (Chart)
- SCHOTT
- RG680 - RG680
- Thickness
- 3.0
- Reflection factor
- 0.9135
Internal Transmittance (Table)
| λ [nm] | |
|---|---|
| 200 | < 10⁻³ |
| 210 | < 10⁻³ |
| 220 | < 10⁻³ |
| 230 | < 10⁻³ |
| 240 | < 10⁻³ |
| 250 | < 10⁻³ |
| 260 | < 10⁻³ |
| 270 | < 10⁻³ |
| 280 | < 10⁻³ |
| 290 | < 10⁻³ |
| 300 | < 10⁻³ |
| 310 | < 10⁻³ |
| 320 | < 10⁻³ |
| 330 | < 10⁻³ |
| 340 | < 10⁻³ |
| 350 | < 10⁻³ |
| 360 | < 10⁻³ |
| 370 | < 10⁻³ |
| 380 | < 10⁻³ |
| 390 | < 10⁻³ |
| 400 | < 10⁻³ |
| 410 | < 10⁻³ |
| 420 | < 10⁻³ |
| 430 | < 10⁻³ |
| 440 | < 10⁻³ |
| 450 | < 10⁻³ |
| 460 | < 10⁻³ |
| 470 | < 10⁻³ |
| 480 | < 10⁻³ |
| 490 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 500 | < 10⁻³ |
| 510 | < 10⁻³ |
| 520 | < 10⁻³ |
| 530 | < 10⁻³ |
| 540 | < 10⁻³ |
| 550 | < 10⁻³ |
| 560 | < 10⁻³ |
| 570 | < 10⁻³ |
| 580 | < 10⁻³ |
| 590 | < 10⁻³ |
| 600 | < 10⁻³ |
| 610 | < 10⁻³ |
| 620 | < 10⁻³ |
| 630 | < 10⁻³ |
| 640 | < 10⁻³ |
| 650 | 0.001 |
| 660 | 0.024 |
| 670 | 0.180 |
| 680 | 0.510 |
| 690 | 0.774 |
| 700 | 0.899 |
| 710 | 0.948 |
| 720 | 0.967 |
| 730 | 0.974 |
| 740 | 0.977 |
| 750 | 0.978 |
| 760 | 0.978 |
| 770 | 0.978 |
| 780 | 0.977 |
| 790 | 0.976 |
| λ [nm] | |
|---|---|
| 800 | 0.976 |
| 810 | 0.975 |
| 820 | 0.975 |
| 830 | 0.974 |
| 840 | 0.974 |
| 850 | 0.974 |
| 860 | 0.973 |
| 870 | 0.973 |
| 880 | 0.973 |
| 890 | 0.973 |
| 900 | 0.973 |
| 910 | 0.973 |
| 920 | 0.973 |
| 930 | 0.973 |
| 940 | 0.973 |
| 950 | 0.973 |
| 960 | 0.973 |
| 970 | 0.973 |
| 980 | 0.973 |
| 990 | 0.973 |
| 1,000 | 0.973 |
| 1,010 | 0.973 |
| 1,020 | 0.973 |
| 1,030 | 0.973 |
| 1,040 | 0.973 |
| 1,050 | 0.973 |
| 1,060 | 0.973 |
| 1,070 | 0.973 |
| 1,080 | 0.974 |
| 1,090 | 0.973 |
| λ [nm] | |
|---|---|
| 1,100 | 0.974 |
| 1,110 | 0.974 |
| 1,120 | 0.974 |
| 1,130 | 0.974 |
| 1,140 | 0.974 |
| 1,150 | 0.975 |
| 1,160 | 0.975 |
| 1,170 | 0.975 |
| 1,180 | 0.976 |
| 1,190 | 0.976 |
| 1,200 | 0.976 |
| 1,250 | 0.978 |
| 1,300 | 0.979 |
| 1,350 | 0.981 |
| 1,400 | 0.983 |
| 1,450 | 0.985 |
| 1,500 | 0.988 |
| 1,550 | 0.989 |
| 1,600 | 0.990 |
| 1,650 | 0.990 |
| 1,700 | 0.989 |
| 1,750 | 0.988 |
| 1,800 | 0.987 |
| 1,850 | 0.985 |
| 1,900 | 0.985 |
| 1,950 | 0.985 |
| 2,000 | 0.984 |
| 2,050 | 0.983 |
| 2,100 | 0.982 |
| 2,150 | 0.979 |
| λ [nm] | |
|---|---|
| 2,200 | 0.970 |
| 2,250 | 0.967 |
| 2,300 | 0.969 |
| 2,350 | 0.970 |
| 2,400 | 0.968 |
| 2,450 | 0.966 |
| 2,500 | 0.964 |
| 2,550 | 0.963 |
| 2,600 | 0.962 |
| 2,650 | 0.957 |
| 2,700 | 0.921 |
| 2,750 | 0.606 |
| 2,800 | 0.426 |
| 2,850 | 0.401 |
| 2,900 | 0.400 |
| 2,950 | 0.397 |
| 3,000 | 0.386 |
| 3,050 | 0.367 |
| 3,100 | 0.346 |
| 3,150 | 0.324 |
| 3,200 | 0.302 |
| 3,250 | 0.282 |
| 3,300 | 0.267 |
| 3,350 | 0.256 |
| 3,400 | 0.253 |
| 3,450 | 0.258 |
| 3,500 | 0.268 |
| 3,550 | 0.282 |
| 3,600 | 0.297 |
| 3,650 | 0.312 |
| λ [nm] | |
|---|---|
| 3,700 | 0.326 |
| 3,750 | 0.338 |
| 3,800 | 0.348 |
| 3,850 | 0.356 |
| 3,900 | 0.363 |
| 3,950 | 0.366 |
| 4,000 | 0.363 |
| 4,050 | 0.352 |
| 4,100 | 0.331 |
| 4,150 | 0.305 |
| 4,200 | 0.277 |
| 4,250 | 0.239 |
| 4,300 | 0.191 |
| 4,350 | 0.142 |
| 4,400 | 0.092 |
| 4,450 | 0.050 |
| 4,500 | 0.023 |
| 4,550 | 0.010 |
| 4,600 | 0.004 |
| 4,650 | 0.002 |
| 4,700 | < 10⁻³ |
| 4,750 | < 10⁻³ |
| 4,800 | < 10⁻³ |
| 4,850 | < 10⁻³ |
| 4,900 | < 10⁻³ |
| 4,950 | < 10⁻³ |
| 5,000 | < 10⁻³ |
| 5,050 | < 10⁻³ |
| 5,100 | < 10⁻³ |
| 5,150 | < 10⁻³ |
Optical values
| Reflection factor | |
|---|---|
| Pd | 0.914 |
| Reference thickness | |
|---|---|
| d [mm] | 3 |
| Spectral values guaranteed | |
|---|---|
| λs (τi = 0.00001) [nm] | 595 nm |
| λc (τi = 0.5) [nm] | 680 nm ± 6 nm |
| λp1 (τi = 0.96) [nm] | 765 nm |
| Refractive Indices n |
|---|
| ns (852.1 nm) = 1.530 |
| nd (587.6 nm) = 1.540 |
Colorimetric evaluation
| Illuminant | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
Physical values
| Density | |
|---|---|
| p [g/cm3] | 2.76 |
| Bubble content | |
|---|---|
| Bubble class | 3 |
| Transformation temperature | |
|---|---|
| Tg [°C] | 532 |
| Temperature coefficient | |
|---|---|
| Tk [nm/°C] | 0.18 |
| Chemical Resistance | |
|---|---|
| FR class | 0 |
| SR class | 1.0 |
| AR class | 1.0 |
| Thermal expansion | |
|---|---|
| α-30°C/+70°C [10-6/K] | 8.1 |
| α20°C/300°C [10-6/K] | 9.4 |
| α20°C/200°C [10-6/K] | |